Show/Hide Menu
Hide/Show Apps
Logout
Türkçe
Türkçe
Search
Search
Login
Login
OpenMETU
OpenMETU
About
About
Open Science Policy
Open Science Policy
Open Access Guideline
Open Access Guideline
Postgraduate Thesis Guideline
Postgraduate Thesis Guideline
Communities & Collections
Communities & Collections
Help
Help
Frequently Asked Questions
Frequently Asked Questions
Guides
Guides
Thesis submission
Thesis submission
MS without thesis term project submission
MS without thesis term project submission
Publication submission with DOI
Publication submission with DOI
Publication submission
Publication submission
Supporting Information
Supporting Information
General Information
General Information
Copyright, Embargo and License
Copyright, Embargo and License
Contact us
Contact us
PRODUCTION OF CRUDE FERRONICKEL FROM SIVRIHISAR LATERITE ORES OF TURKEY
Date
2013-03-07
Author
KESKİNKILIÇ, ENDER
Pournaderi, Saeid
Geveci, Ahmet
Topkaya, Yavuz Ali
Metadata
Show full item record
This work is licensed under a
Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International License
.
Item Usage Stats
205
views
0
downloads
Cite This
In the current work, laboratory-scale smelting experiments were conducted using Sivrihisar laterites (1.26% Ni). The ore samples previously subjected to drying, calcination and prereduction stages were smelted in alumina crucibles in a horizontal tube furnace under argon atmosphere. For the smelting system used in the present work, 1550 degrees C and 40 minutes were determined to be the optimum smelting temperature and time, respectively. 25% excess coal addition in prereduction stage was reported to be crucial to obtain the desired Ni content in the final product. Colemanite in calcined form has long been known as a flux used in pyrometallurgical systems such as steelmaking and copper matte-smelting. To investigate the effects of calcined colemanite addition on the ferronickel metal-slag system, calcined colemanite of 2% and 4% of the total metal and slag weight was charged as a flux and smelted under the optimum conditions described above.
Subject Keywords
Smelting
,
Laterite
,
Ferronickel
URI
https://hdl.handle.net/11511/55558
Collections
Graduate School of Natural and Applied Sciences, Conference / Seminar
Suggestions
OpenMETU
Core
STUDY OF CERTAIN PARAMETERS IN LABORATORY-SCALE SMELTING OF SIVRIHISAR LATERITE ORES OF TURKEY
KESKİNKILIÇ, ENDER; Pournaderi, Saeid; Geveci, Ahmet; Topkaya, Yavuz Ali (2012-03-15)
Conventional ferronickel smelting has five main steps: Drying, calcination, prereduction, smelting and refining. In the scope of the current work, smelting experiments were conducted using Sivrihisar laterite ores (1.26% Ni) of Turkey. The ore samples previously subjected to drying, calcination and prereduction stages were smelted in alumina crucibles in a laboratoryscale horizontal tube furnace under argon atmosphere. Smelting experiments were performed at 1500, 1550 and 1600 degrees C. The amount of exces...
USE OF COLEMANITE IN FERRONICKEL SMELTING
KESKİNKILIÇ, ENDER; Pournaderi, S.; Geveci, Ahmet; Topkaya, Yavuz Ali (2019-01-01)
Use of colemanite in metal-slag systems aims primarily to decrease the viscosity of slag and, therefore, achieve better metal-slag separation. Enhanced metal-slag separation is helpful to decrease the number of suspended metal/alloy droplets in slag, i.e. the physical losses. In the literature, successful use of colemanite was reported both in steelmaking and copper matte smelting processes. Ferronickel smelting slags contain nickel in the range of 0.1-0.2% and correspondingly, metal-slag distribution ratio...
Determination of deep trapping center parameters in as-grown Tl2Ga2S3Se layered crystals
YILDIRIM, TACETTİN; Hasanlı, Nızamı (Elsevier BV, 2009-09-01)
Thermally stimulated current measurements were carried out on as-grown Tl2Ga2S3Se layered single crystals. The investigations were performed in temperatures ranging from 10 to 320 K with heating rates of 0.6-1.2 K s(-1). The analysis of the data revealed the hole trap level located at 498 meV. The activation energies of the traps have been determined using various methods of analysis, and they agree with each other. The calculation for these traps yielded 2.1 x 10(-18) cm(2) for capture cross-section and 2....
Processing and characterization of high density tungsten-nickel-iron alloys
Çalışkan, Necmettin Kaan; Bor, Şakir; Durlu, Nuri; Department of Metallurgical and Materials Engineering (2013)
In the present study, processing of W-Ni-Fe alloys by liquid phase sintering technique has been investigated. Effect of sintering atmospheres (hydrogen and vacuum), tungsten content altering from 90 to 97 wt.%, Ni/Fe ratio varied from 2 to 4 and post sintering treatments (heat treatment and swaging) on the microstructure and mechanical properties of W-Ni-Fe alloys have been analyzed. Liquid phase sintered alloys were characterized by mechanical tests, electron microscopy and XRD studies, thermal analyses an...
Growth and characterization of NaBi(Mo0.5W0.5O4)2 single crystal: A promising material for optoelectronic applications
Isik, M.; Guler, I.; Hasanlı, Nızamı (2023-03-15)
The structural and optical characteristics of NaBi(Mo0.5W0.5O4)2 single crystals grown by Czochralski method were investigated. X-ray diffraction (XRD) pattern exhibited four well-defined peaks related to tetragonal crystalline structure with a space group I41/a. Raman and infrared transmittance spectra were recorded to investigate vibrational properties of the compound. Room temperature transmission spectrum was measured to reveal band gap energy of the crystal. The derivative spectral and absorption coeff...
Citation Formats
IEEE
ACM
APA
CHICAGO
MLA
BibTeX
E. KESKİNKILIÇ, S. Pournaderi, A. Geveci, and Y. A. Topkaya, “PRODUCTION OF CRUDE FERRONICKEL FROM SIVRIHISAR LATERITE ORES OF TURKEY,” 2013, Accessed: 00, 2020. [Online]. Available: https://hdl.handle.net/11511/55558.